Mostrar el registro sencillo del ítem
Propiedades magnéticas del sistema de aleaciones Cu2Cd1-ZMnZSnSe4
dc.rights.license | http://creativecommons.org/licenses/by-nc-sa/3.0/ve/ | es_VE |
dc.contributor.author | Moreno, E. | |
dc.contributor.author | Quintero, M. | |
dc.contributor.author | Morocoima, Manuel J. | |
dc.contributor.author | Villarreal, Manuel | |
dc.contributor.author | Quintero, E. | |
dc.contributor.author | Grima Gallardo, Pedro | |
dc.contributor.author | Tovar, R. | |
dc.contributor.author | Caldera Moreno, Dayana Carolina | |
dc.contributor.author | Álvarez, S. | |
dc.contributor.author | Bocaranda, Pablo | |
dc.contributor.author | Henao, J. A. | |
dc.contributor.author | Macías, M. A. | |
dc.date.accessioned | 2019-05-29T13:57:42Z | |
dc.date.available | 2019-05-29T13:57:42Z | |
dc.date.issued | 2019-05-29 | |
dc.identifier.issn | pISSN: 0255-6952 | |
dc.identifier.uri | http://www.saber.ula.ve/handle/123456789/45787 | |
dc.description.abstract | En este trabajo se reportan las medidas de susceptibilidad magnética X en función de la temperatura en el rango de 2-300 K de muestras policristalinas del sistema de aleaciones semiconductor magnético Cu2Cd1-zMnzSnSe4. La constante de Curie C aumenta linealmente con la concentración z. La temperatura de Curie-Weiss 0 y la temperatura de Néel TN aumentan linealmente con la concentración z, debido a un cambio de orden parcial a desorden total de los átomos de Mn2+ en el sistema. En una primera aproximación, se puede considerar que el sistema de aleaciones tiene un comportamiento típico de vidrio de espín, lo que implica que los iones de Mn2+ se encuentran de alguna manera desordenados en la red catiónica del material. | es_VE |
dc.language.iso | es | es_VE |
dc.publisher | SaberULA | es_VE |
dc.rights | info:eu-repo/semantics/openAccess | es_VE |
dc.subject | Aleaciones semiconductoras magnéticas | es_VE |
dc.subject | Susceptibilidad magnética | es_VE |
dc.subject | Vidrio de espín | es_VE |
dc.title | Propiedades magnéticas del sistema de aleaciones Cu2Cd1-ZMnZSnSe4 | es_VE |
dc.type | info:eu-repo/semantics/article | es_VE |
dcterms.dateAccepted | 26-01-2018 | |
dcterms.dateSubmitted | 10-07-2017 | |
dc.description.abstract1 | Measurements of magnetic susceptibility ? as a function of temperature in the range 2-300 K on polycrystalline samples of Cu2Cd1-zMnzSnSe4 magnetic semiconductor alloy system are reported. The Curie constant C increase linearly with z. The Curie-Weiss temperature ? and Néel temperature TN increase linearly with z due to a partial order change to total disorder of the Mn+2 ions in the system. In a first approximation, it can be considered that this system has typical spin glass behavior (spin glass system), which means that ions Mn+2 are somewhat disorderly way cationic network of material. | es_VE |
dc.description.colacion | 1-7 | es_VE |
dc.description.email | moroco@ula.ve | es_VE |
dc.description.email | mavu@ula.ve | es_VE |
dc.description.email | peg@ula.ve | es_VE |
dc.description.email | calderad@ula.ve | es_VE |
dc.identifier.eissn | eISSN: 2244-7113 | |
dc.subject.facultad | Facultad de Ciencias | es_VE |
dc.subject.institucion | Universidad de Los Andes | es_VE |
dc.subject.keywords | Magnetic semiconductor alloys | es_VE |
dc.subject.keywords | Magnetic susceptibility | es_VE |
dc.subject.keywords | Spin glass | es_VE |
dc.subject.thematiccategory | Física | es_VE |
dc.subject.tipo | Artículos | es_VE |
dc.subject.unidadinv | 1 Centro de Estudios de Semiconductores, Departamento de Física, Universidad de Los Andes, Facultad de Ciencias,Apartados de Correos No.1, La Hechicera-Mérida 5251, Venezuela. 2 Grupo de Investigación en Química Estructural,Escuela de Química, Universidad Industrial de Santander, Facultad de Ciencias, Apartado Aéreo 678, Bucaramanga,Colombia. | es_VE |
dc.type.media | Texto | es_VE |